MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch® 8624 Tear Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® Tear Tape 8624 is a designed for use as the easy-opening device on paperboard and light- to medium-weight corrugated fiberboard packaging materials. Typical easy-opening applications for Scotch® Tape 8624 include: overnight courier envelopes; overnight courier boxes; audio/video/CD/book mailers; printed boxes used in the retail market for such items as electronics, toys, medical, computers, and clothing; and shipping boxes used by catalogs and “mail order” retailers, who want to avoid product damage from knives, razor blades and scissors used to open the packages.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 114 microns4.50 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.6 MPa3560 psiASTM D3759
Elongation at Break 30 %30 %ASTM D3759
Peel Strength 0.71216 kN/m4.0625 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypePressure sensitive synthetic rubber resin
AppearanceBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch® 231A Performance Masking Tape
3M Scotch® 231 Performance Masking Tape
3M Scotch® 226 Solvent Resistant Masking Tape
3M Scotch® 222 High-temperature Fine Line Masking Tape
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape

PMM34238 / 168985

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.