MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Tuflin™ HS-7098D NT 7 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Product Description: Tuflin™ HS-7098D NT 7 ethylene-hexene copolymer, LLDPE resin designed for cast and blown film applications such as trash bags, industrial can liners, and retail bags. Films extruded with HS-7098D NT 7 exhibit superb toughness, high tensile strength and elongation, excellent tear and puncture resistance, and are readily heat sealable.
Main Characteristics:
  • Hexene Linear Low Density Resin
  • High toughness
  • High strength
  • Compiles with US FDA 21 CFR 177.1520©3.1a
Application: Heavy Duty Industrial and Consumer Liners

Availability: North America

Agency Ratings: FDA 21 CFR 177.1520(c)3.1a

Additive: Antiblock: 2500 ppm; Processing Aid: No; Slip: 1000 ppm

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 2500 ppm2500 ppm
Slip Level 1000 ppm1000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %
@Thickness 0.0254 mm
500 %
@Thickness 0.00100 in
ASTM D882
Film Elongation at Break, TD 700 %
@Thickness 0.0254 mm
700 %
@Thickness 0.00100 in
ASTM D882
Elmendorf Tear Strength MD 310 g
@Thickness 0.0254 mm
310 g
@Thickness 0.00100 in
Method B; ASTM D1922
Elmendorf Tear Strength TD 800 g
@Thickness 0.0254 mm
800 g
@Thickness 0.00100 in
Method B; ASTM D1922
Dart Drop Test 200 g
@Thickness 0.0254 mm
0.441 lb
@Thickness 0.00100 in
F50; ASTM D1709A
Film Tensile Strength at Break, MD 44.8 MPa
@Thickness 0.0254 mm
6500 psi
@Thickness 0.00100 in
ASTM D882
Film Tensile Strength at Break, TD 34.5 MPa
@Thickness 0.0254 mm
5000 psi
@Thickness 0.00100 in
ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 16 %
@Thickness 0.0254 mm
16 %
@Thickness 0.00100 in
ASTM D1003
Gloss 45 %
@Thickness 0.0254 mm
45 %
@Thickness 0.00100 in
45°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 231 °C448 °FExtrusion
Blow-up Ratio (BUR) 2.52.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF567 / 311260

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.