MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor™ 19MB440 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.

Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South America

Key Features:

  • Very good sealability of the untreated surface with a wide range of polyethylene for lap seal applications
  • Excellent jaw release
  • Outstanding optical properties, stable in time
Features:
  • In Lamination Lap Sealable
  • Lap Sealable to PE
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Fresh Produce
  • Frozen Food
  • Health and Beauty Care
  • Household and Detergents
  • Ice Cream
  • Pet food
Uses:
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing and Solvent Rotogravure Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.0900 g/100 in²/day
@Temperature 23.0 °C
85% RH; ExxonMobil Method
 0.450 g/100 in²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Thickness 0.750 milExxonMobil Method
Coating Weight 10.6 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 175 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 45 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 290 ksiMD; ExxonMobil Method
 580 ksiTD; ExxonMobil Method
Coefficient of Friction 0.40Untreated Surface; ExxonMobil Method
Seal Strength 510 g/in
@Pressure 0.276 MPa,
Temperature 140 °C
Otto Bruger, 0.2 sec; ExxonMobl Method
 810 g/in
@Pressure 0.276 MPa,
Temperature 140 °C
Otto Bruger, 0.2 sec; ExxonMobl Method
Film Tensile Strength at Break, MD 18100 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 41300 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
Shrinkage, TD 4.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ExxonMobil Method
Gloss 85 %45°; ExxonMobil Method
 
Descriptive Properties
Heat Seal Range15°CUT/LLDPE, 36.3 psi (0.25 MPa), 0.2 sec
 25°CUT/LLDPE, 36.3 psi (0.25 MPa), 0.2 sec
Yield40600 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C15760

PEX99452 / 175688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.