MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Elvax® resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range without the need for plasticizers.

Elvax® resins can be used alone or to improve the flexibility, resilience and toughness of other resins. Depending on the demands of the particular application, they can be pigmented, foamed, filled, and/or crosslinked. In addition to their performance advantages, Elvax® resins are processed easily using conventional thermoplastic processing techniques, i.e., injection molding, extrusion and foaming, as well as rubber processing techniques, i.e., Banbury mixing, foam extrusion and molding.

Test specimens except for tensile impact where prepared by compression molding (ASTM D1928, procedure C). Tensile impact samples were injection molded.

Processing Information:

Molding and Extruding

Modified and unmodified Elvax® resins can be processed in conventional thermoplastic and rubber processing equipment. The temperature profile will vary with machine type, size and screw design as well as with part size, thickness or configuration.

Compounding

Elvax® resins are compatible with a variety of other resins and elastomers including polyethylene, polypropylene and styrene-butadiene rubber. Clays and other inorganic fillers can be added to improve abrasion resistance and lower cost.

Foaming Agents

Elvax® resins are readily foamed using chemical or physical blowing agents.

Crosslinking Agents

Peroxides such as "Di-Cup"† and "Vul-Cup"† dicumyl peroxide can be used to crosslink or vulcanize Elvax® resins.

(†Hercules Inc.)

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Vinyl Acetate Content 15 %TGA
Melt Index of Compound 2.5 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98ASTM D2240
Hardness, Shore D 47ASTM D2240
Tensile Strength, Ultimate 19.0 MPaType IV, crosshead speed 2 in/min; ASTM D638
 12.0 MPa
@Temperature 49.0 °C
Type IV, crosshead speed 2 in/min; ASTM D638
 32.0 MPa
@Temperature -20.0 °C
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
Elongation at Break 650 %Type IV, crosshead speed 2 in/min; ASTM D638
 500 %
@Temperature -20.0 °C
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
 750 %
@Temperature 49.0 °C
Type IV, crosshead speed 2 in/min; ASTM D638
Modulus of Elasticity 0.0960 GPa
 0.345 GPa
@Temperature -20.0 °C
Flexural Modulus 0.110 GPaASTM D790
 0.0530 GPa
@Temperature 49.0 °C
ASTM D790
 0.503 GPa
@Temperature -20.0 °C
ASTM D790
Flexural Stiffness 13920 psi
 50040 psi
Tensile Impact Strength 425 kJ/m²
@Temperature -20.0 °C
ASTM D1822
 450 kJ/m²
@Temperature 23.0 °C
ASTM D1822
Compression Set 84 %
@Temperature 70.0 °C
Method B, 22 hours; ASTM D395
 52 %
@Temperature 25.0 °C,
Time 864000 sec
Method B; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 80.0 °CASTM D1525
Brittleness Temperature <= -100 °CASTM D762
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 - 204 °C
 
Descriptive Properties
Cycle time0.5-2 minutesMolding, equipment and part design dependent
Vinyl Acetate Content15 wt.%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 410 Ethylene Vinyl Acetate
Dow Elvax® 440 Ethylene Vinyl Acetate
Dow Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin

PDUPM130 / 33797

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.