MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Plastolyn™ 240 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: Plastolyn™ 240 hydrocarbon resin is a versatile, aromatic, water white, high softening point resin for use in polymer modification, adhesives, overprint lacquers, coatings and a variety of other applications. Recommended as a flow modifier in such polymers as polyvinylchloride (PVC), acrylonitrile-butadiene-styrene (ABS) and block copolymers. Its water white color and good economy, combined with superior heat and ultraviolet light (UV) stability compared with conventional C9 hydrocarbon resins, provide formulators a new level of quality without sacrificing competitiveness.

Application/Uses:

  • Automotive
  • Building and Construction
  • Contact Adhesives
  • Hot Melt Adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
Key Attributes:
  • Color stability
  • High softening point
  • Low color
  • Made from purified aromatic monomers

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 197 °C
Melt
 10000 cP
@Temperature 161 °C
Melt
 100000 cP
@Temperature 140 °C
Melt
Molecular Weight 1550 g/molMn
 4060 g/molMw. Mw/Mn ratio = 2.6
 7600 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 72.0 °C
Ring & Ball Softening Point 120 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point<-50°CDACP
 >180°COMS
 9°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed bar
Arkema Nakan® FKS 911 S PVC, Soft Extrusion Grade
Nitinol - NiTi Shape Memory Alloy; Low-Temperature Phase
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Geon® Performance Solutions 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

PEATM5533 / 222727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.