MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay FF05AP
Categories: Other Engineering Material

Material Notes: Description: Combination product. Ideally suited to medium temperature applications.

Features & Benefits:

  • PTFE coated glass fabric tool release sheet for lining molds to give a durable, non contaminating release surface
  • Also used to cover patterns prior to the lay up of composite molds
  • Supplied with a pressure sensitive, adhesive backing
  • Self-adhesive back PTFE coated glass fabrics can only be applied in one piece to flat or single curvature tooling. However, the material can be effectively butt jointed on complex tooling.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 4.50 - 5.50 microns0.177 - 0.217 milAdhesive
 122 microns4.80 milFabric
 172 microns6.77 milThickness
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °FAcrylic
 260 °C500 °FSilicone
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCYTED223 / 180525

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.