MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® 2S 25 W 20 X nat PA610-I
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and its eco-profile is very favorable when compared to similar products based on crude oil. The main feature of Grilamid 2S 25 W 20 X natural:
  • High impact strength, even at low temperatures
  • High heat resistance
  • Good chemical resistance
  • Easy processing
GRILAMID 2S 25 W 20 X natural can be processed on al standard tube-extrusion lines suitable for polyamides.

Application examples: Preferred applications are flexible tubes in the fields of Automotive and Industry.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccDry; ISO 1183
Water Absorption 3.0 %Sim. to ISO 62
Moisture Absorption 0.500 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.023 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.017 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 35.0 MPaConditioned; ISO 2039-1
 50.0 MPaDry; ISO 2039-1
Tensile Strength at Break 40.0 MPaDry; ISO 527-1/-2
 40.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 >= 50 %Conditioned; ISO 527-1/-2
Tensile Modulus 450 MPaConditioned; ISO 527-1/-2
 750 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 37.0 kV/mmConditioned; IEC 60243-1
 38.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 200 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°CISO 11359-1/-2
Melting Point 215 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 - 130 °CLong Term; ISO 2578
 170 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AdditivesPlasticizer
AutomotiveAir intake systems
 Compressed air systems
 Fuel systems
 Hydraulic systems
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
 Profile Extrusion
Product AttributesBio based Polyamide
 Flexible
 High viscosity
Special CharacteristicsHigh impact or impact modified
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® 2D 25 W 20 X nat PA612-I
EMS-Grivory Grilamid® 2D 25 W 20 X black PA612-I
EMS-Grivory Grilamid® 2D 25 W 20 HL X black 9992 PA612-I
Teknor Apex Chemlon 253 H Nylon 6, Impact Modified
EMS-Grivory Grilamid® XE 4071 nat PA612-I

PGRH016 / 156725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.