MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite Durez® 32340 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez® 32340 is a phenolic novolac in solution for use in the refractory industry like the production of crucibles. Viscosity can vary from 5000 up to 20000 cps depending on the water content and solids. Addition of hexamethylenetetramine is necessary to make it thermosetting.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 80 %80 %DCT 156
Water Absorption 2.3 %2.3 %DCT 74
Viscosity Measurement 16000
@Temperature 25.0 °C
16000
@Temperature 77.0 °F
DCT 61
 
Descriptive Properties
Free Phenol, %0.8DCT 431

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Plyophen 43575 Phenolic Resin
Sumitomo Bakelite Plyophen 23900 Phenolic Resin
Sumitomo Bakelite Durez® 33840 Phenolic Resin
Sumitomo Bakelite Durez® 32341 Phenolic Resin
Sumitomo Bakelite Durez® 28391 Phenolic Resin

PSUMIT258 / 194063

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.