MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Saint-Gobain Norton® Tygon® 2075 Ultra Chemical Resistant Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Replaced by Tygon® S3 2075. Description: Tygon® 2075: Tygon® Ultra Chemical Resistant Tubing offers an unequaled combination of chemical resistance, clarity and flexibility. Tygon® Ultra Chemical Resistant Tubing is virtually unaffected by acids, bases, ketones, salts and alcohols, fitting the requirements of many applications from battery acid filling to hazardous material handling. It's entirely plasticizer-free, eliminating fluid contamination and the premature embrittlement and cracking common with many flexible tubings. Its exceptionally smooth inner surface inhibits particulate buildup and reduces the potential for contamination.

Features/Benefits:
  • Resistant to MEK and other highly aggressive chemicals
  • Plasticizer free
  • Safer disposal through incineration
  • Smoother inner surface inhibits particulate build-up
  • Hydrophobic property reduces absorption of aqueous fluids
  • Minimal outgassing from tubing protects sensitive environments
  • Documented biocompatibility to the ISO 10993 standard
  • Meets USP Class VI criteria and FDA requirements for food contact.
Typical applications include Fine and Specialty Chemical Production, Battery Acid Filling, Clean and Degreaser Transfer Systems, X-ray Processing, Paint and Solvent Production, Ink and Printing Fluid Dispensing, Hazardous Materials Handling, Power Generation Sampling and Drain Lines
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792-98
Water Absorption <= 0.010 %24 hours at 23°C; ASTM D570-98
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7215 seconds; ASTM D2240-97
Tensile Strength, Yield 2000 psiASTM D412-98
Elongation at Break 700 %ASTM D412-98
100% Modulus 0.350 ksi
@Strain 100 %
ASTM D412-98
Tear Strength 220 pliInitial Tear Strength; ASTM D1004-94
Compression Set 84 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-98 Method B
Tensile Set 187 %ASTM D412-98
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 587 V/milASTM D149-97
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °F
Brittleness Temperature -108 °FASTM D746-98
 -94.0 °FLow Temperature Flexibility; ASTM D381-94
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® Tygon® R-1000 Ultra-Soft Tubing Formulation
Saint-Gobain Tygon® 2275 High Purity Tubing Formulation
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation
Saint-Gobain Tygon® LP 1500 Low Permeation Fuel Tubing

PSTGQZ196 / 68710

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.