MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS Tristar® PC-09FRN-WT 10 MFI Flame Retardant Polycarbonate With Release  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Water Absorption 0.18 %24 hours at 73°F; ASTM D570
Linear Mold Shrinkage 0.005 - 0.007 cm/cmASTM D955
Melt Flow 9.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 59.0 MPa
@Thickness 3.17 mm
ASTM D638
Elongation at Break 100 %
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 75.0 MPa
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 2.07 GPa
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 7.00 J/cm
@Thickness 3.17 mm
ASTM D256
Tensile Impact Strength 211 ft-lb/in²
@Thickness 3.17 mm
ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3e+15 ohm-cm50% RH, 96 hours @ 90°C; ASTM D257
 6e+15 ohm-cm50% RH; ASTM D257
Dielectric Strength 24.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Arc Resistance 64 sec3.3 mm; ASTM D495
High Voltage Arc Resistance to Ignition (HVAR) 16 sec
@Thickness 1.60 mm
UL746A
Comparative Tracking Index 250 V3.3 mm; ASTM D3638
Hot Wire Ignition, HWI 20 sec
@Thickness 1.62 mm
ASTM D3874
 41 sec
@Thickness 3.00 mm
ASTM D3874
High Amp Arc Ignition, HAI 108 arcs
@Thickness 3.00 mm
50% RH; UL746A
 142 arcs
@Thickness 1.62 mm
50% RH; UL746A
High Voltage Arc-Tracking Rate, HVTR 103 mm/min3.0 mm; UL746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °CASTM D648
UL RTI, Electrical 125 °C3.0 mm
UL RTI, Mechanical with Impact 115 °C3.0 mm
UL RTI, Mechanical without Impact 125 °C3.0 mm
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VA
@Thickness 2.10 mm
white
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 510 - 530 °F
Middle Barrel Temperature 520 - 540 °F
Front Barrel Temperature 540 - 570 °F
Nozzle Temperature 530 - 580 °F
Melt Temperature 550 - 600 °F
Mold Temperature 160 - 200 °F
Drying Temperature 250 °F
Dry Time 3 - 4 hour48 hours max.
Injection Pressure 12000 - 18000 psi
Back Pressure 50.0 - 200 psi
Clamp Pressure 4000 - 10000 psi
Shot Size 40 - 60 %
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Injection Speed- Edge GateSlow to Medium
Injection Speed- Tab GateMedium to Fast
Injection Speed- Tunnel GateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZ9PT83m / 146988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.