MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) TEDUR® L 9107-1 PPS, 40% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Base Polymer: Polyphenylene Sulfide

Filler/Additive System: 40% glass fibers

Special Features: Injection molding grade, high toughness, reduced flash, increased burst strength

Application Area: Pump components

Typical Applications: Pump impellers

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³ISO 1183
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiISO 527
Elongation at Break 1.7 %1.7 %ISO 527
Tensile Modulus 15.0 GPa2180 ksiISO 527
Flexural Strength 260 MPa37700 psiISO 178
Flexural Modulus 13.5 GPa1960 ksiISO 178
Flexural Strain at Break 2.2 %2.2 %Flexural deflection at max force; ISO 178
Izod Impact, Unnotched (ISO) 50.0 kJ/m²23.8 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 5.50 J/cm²26.2 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN EN 62631-3-2
Comparative Tracking Index 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357
Vicat Softening Point 270 °C518 °FA50; ISO 306
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
passed; DIN EN 60695
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °FInjection molding
Mold Temperature >= 140 °C>= 284 °FInjection molding
Drying Temperature 130 - 140 °C
@Time 7200 - 14400 sec
266 - 284 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyphenylene Sulfide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) TEDUR® L 9510-1 PPS, 40% Glass Fiber Reinforced
Mocom (ALBIS) TEDUR® L 9107-7 PPS, 40% Glass Fiber Reinforced
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber

PALBIS8343 / 242402

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.