MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Sandvik Sanicro 70 Seamless tube and pipe
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Nickel-chromium-iron-alloy, UNS N06600

Sandvik Sanicro 70 is an austenitic nickel-chromium-iron alloy, characterized by very good resistance to carburization and nitrogen absorption and good structural stability at high temperatures. It has also good resistance to stress corrosion cracking.

Information provided by Sandvik

UNS N06600; EN 2.4816

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160cold/hot finished
Tensile Strength, Ultimate 550 - 700 MPahot finished
 552 - 700 MPacold finished
 >= 440 MPa
@Temperature 600 °C
 >= 450 MPa
@Temperature 500 °C
 >= 460 MPa
@Temperature 400 °C
 >= 470 MPa
@Temperature 300 °C
 >= 500 MPa
@Temperature 100 °C
 >= 500 MPa
@Temperature 200 °C
Tensile Strength, Yield >= 205 MPa
@Strain 0.2 %
cold finished
 >= 230 MPa
@Strain 1 %
hot finished
 >= 241 MPa
@Strain 0.2 %
cold finished
 >= 265 MPa
@Strain 1 %
hot finished
 >= 100 MPa
@Strain 0.2 %,
Temperature 600 °C
 >= 140 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 160 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 170 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 180 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 200 MPa
@Strain 0.2 %,
Temperature 100 °C
Elongation at Break >= 35 %cold/hot finished
Modulus of Elasticity 214 GPa
 135 GPa
@Temperature 1000 °C
 149 GPa
@Temperature 900 °C
 161 GPa
@Temperature 800 °C
 171 GPa
@Temperature 700 °C
 180 GPa
@Temperature 600 °C
 185 GPa
@Temperature 500 °C
 190 GPa
@Temperature 400 °C
 196 GPa
@Temperature 300 °C
 202 GPa
@Temperature 200 °C
 206 GPa
@Temperature 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.5 µm/m-°C
@Temperature 30.0 - 100 °C
 14.0 µm/m-°C
@Temperature 30.0 - 200 °C
 14.0 µm/m-°C
@Temperature 30.0 - 300 °C
 14.5 µm/m-°C
@Temperature 30.0 - 400 °C
 15.0 µm/m-°C
@Temperature 30.0 - 500 °C
 15.0 µm/m-°C
@Temperature 30.0 - 500 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.480 J/g-°C
@Temperature 100 °C
 0.495 J/g-°C
@Temperature 200 °C
 0.510 J/g-°C
@Temperature 300 °C
 0.515 J/g-°C
@Temperature 400 °C
 0.525 J/g-°C
@Temperature 500 °C
 0.590 J/g-°C
@Temperature 600 °C
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 °C
 14.0 W/m-K
@Temperature 100 °C
 16.0 W/m-K
@Temperature 200 °C
 17.0 W/m-K
@Temperature 300 °C
 19.0 W/m-K
@Temperature 400 °C
 21.0 W/m-K
@Temperature 500 °C
 25.0 W/m-K
@Temperature 600 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.050 %
Chromium, Cr 16.5 %
Copper, Cu <= 0.50 %
Iron, Fe <= 10 %
Manganese, Mn 0.80 %
Nickel, Ni 72.5 %
Phosphorus, P <= 0.015 %
Silicon, Si 0.40 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV253 / 19147

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.