MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec ALUTIT® T Aluminum Titanate (Thermal Shock Optimized)
Categories: Ceramic; Oxide; Aluminum Oxide; Titanium Oxide

Material Notes: ALUTIT®, which is produced in a special reaction-sintering process, consists of high-purity aluminum oxide and titanium oxide. It offers excellent resistance to sudden changes in temperature, good heat insulation, low thermal expansion, and good chemical resistance. Typical applications are found in the nonferrous metals casting industry. ALUTIT® T offers good thermal shock resistance and is used primarily in components subject to high thermal loads, e.g., as hot top rings, breakings, and nozzles.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.35 g/cc
Porosity 12.5 %
Pore Size >= 0.200 micronsAverage Radius
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 17.0 GPa
Flexural Strength 25.0 MPaBending Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear <= 1.00 µm/m-°C
@Temperature 20.0 - 600 °C
Thermal Conductivity 1.50 W/m-K
 
Descriptive Properties
Thermal Shock Resistance R1 (K)> 1000maximum air/fluid temperature gradient

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec ALUTIT® S Aluminum Titanate (Strength Optimized)
3M Techical Ceramics Ekatherm® Silicon Nitride
Pyrotek O'-Sialon Non-Oxide Ceramic
Titanium Dioxide, Rutile
CoorsTek PlasmaPure™ AD-998 Alumina (nom. 99.8% Al2O3)

CCERA964 / 107564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.