MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubriplate FGL CC Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: High performance, multi-purpose food grade grease designed to meet the demands of food and beverage industry plant engineers who want Class H-1 greases to totally replace H-2 greases. Fortified with anti-wear, anti rust and anti-corrosion additives which combine to yield excellent shear stability, load carrying capability and resistance to water and caustic wash down. Available in four NLGI densities for a variety of applications. FGL-CC is for centralized/automatic lubrication systems on high speed can closing equipment.

FGL Series greases are available in Cans, Pails, 1/4 Drums and Drums. FGL-1 and FGL-2 are available in Cartridges.

H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.

Information provided by Lubriplate

Key Words: Part Number L0229-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 550 SUS
Kinematic Viscosity at 40°C (104°F) 120 cSt
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 370Unknown Amount of Work
Penetration P(60), 1/10 mm 410Unknown Amount of Work
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air 0.000 °FApprox. Cold test
Dropping Point 450 °FASTM Test
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW
NLGI Grade0/00
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WLUBR175 / 76221

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.