MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reade Advanced Materials Diopside Powder (CaMg(CO3)2 and CaMg(SiO3)2)
Categories: Ceramic

Material Notes: Description: A naturally mined mineral that is relatively difficult to source. Low-iron grades have use in glass manufacture, whiteware bodies, glazes, and welding rod coatings.
Forms Available: Lump or powder (100 mesh x down, 250 mesh by down or 400 mesh by down)

Information provided by Reade Advanced Materials.

Key Words: CaMg(CO3)2 and CaMg(SiO3)2, Calcium-magnesium silicate, calcium-magnesium pyroxene, malacolite, alalite
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.20 - 3.38 g/cc
Density 204.8 lb/ft³

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borosilicate Glass
Corning Gorilla® Glass 5 Display Glass
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
Celanese Zenite® 5145L BK010 LCP
Cancarb Thermax® Powder N908 Stainless Medium Carbon Black

CREADE009 / 1943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.