MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed colored.

Applications:Typical applications include those requiring weatherability and toughness for automotive exterior applications and lawn and garden applications. As with any product, use of Diamaloy GLY 7510 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 8.3 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 101ASTM D785
Tensile Strength at Break 38.0 MPachs 2.0 in/min; ASTM D638
Tensile Strength, Yield 52.0 MPachs 2.0 in/min; ASTM D638
Elongation at Break 22 %chs 2.0 in/min; ASTM D638
Elongation at Yield 3.0 %chs 2.0 in/min; ASTM D638
Tensile Modulus 2784 MPachs 2.0 in/min; ASTM D638
Flexural Strength 79.0 MPa
@Thickness 3.17 mm
chs 0.05 in/min; 2 in span; ASTM D790
Flexural Modulus 2432 MPa
@Thickness 3.17 mm
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 42.7 J/m
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D256
 246 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
Instrumented Impact Total Energy 20.8 J
@Temperature -30.0 °C
ASTM D3763
 27.0 J
@Temperature 23.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Hot Wire Ignition, HWI 3.0 secPLC Code; ASTM 746A
High Amp Arc Ignition, HAI 0.00 arcsPLC Code; ASTM 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µin/in-°F
@Temperature -40.0 - 37.8 °C
ASTM E831
CTE, linear, Transverse to Flow 48.0 µin/in-°F
@Temperature -40.0 - 37.8 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 102 °C0.125";; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C0.125";; ASTM D648
Vicat Softening Point 104 °CASTM D1525
Flammability, UL94 HB
@Thickness 1.52 mm
 
Optical PropertiesOriginal ValueComments
Gloss 94 %Untextured; 60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
Trinseo Plexiglas® V825 Acrylic
INEOS Styrolution Luran® S KR 2859 ASA
A. Schulman Diamond ASA S210B
A. Schulman Diamond Centrex® 810 Injection Molding Grade

PDIAM398 / 126489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.