MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Estane® D91T86 NAT 01 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Aliphatic polycaprolactone based Thermoplastic Polyurethane (TPU) with a 88 Shore A Hardness.

Features: Translucent resin with excellent colour stability upon UV exposure

Uses: Injection molding outdoor applications. Preliminary data.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccISO 2781 / ASTM D-792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88
@Time 3.00 sec
ISO 868
Tensile Strength 34.0 MPaISO 527-2 / ASTM D-412
Elongation, Ultimate 700 %ISO 34-1B (ASTM D-624 Die C)
100% Modulus 6.00 MPa
@Strain 100 %
ISO 527-2 / ASTM D-412
300% Modulus 9.00 MPa
@Strain 300 %
ISO 527-2 / ASTM D-412
Tear Strength 110 kN/mISO 527-2 / ASTM D-412
Abrasion 20[mm3]; ISO 4649
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 86.0 °CA50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 25 %
@Thickness 2.00 mm
ASTM 1003
 
Processing PropertiesOriginal ValueComments
Feed Temperature 170 °C
Nozzle Temperature 185 °C
Zone 2 175 °C
Zone 3 180 °C
Mold Temperature 35.0 °C
Drying Temperature 90.0 °C
@Time 7200 sec
Moisture Content <= 0.10 %MQSA 44
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5021 / 238891

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.