MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 4002 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D 792
Filler Content 15 %Primary Additive
Water Absorption 0.26 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 125ASTM D 785
Tensile Strength at Break 14000 psiASTM D 638
Elongation at Break 1.0 - 2.0 %ASTM D 638
Tensile Modulus 900 ksiASTM D 638
Flexural Strength 22000 psiASTM D 790
Flexural Modulus 800 ksiASTM D 790
Izod Impact, Notched 0.800 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 5.00 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 3.9
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 500 °FASTM D 648
Flammability, UL94 HB
@Thickness 0.7937 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 625 - 650 °F
Mold Temperature 150 - 325 °F
Drying Temperature 225 °F
Dry Time 4 - 6 hour
Moisture Content 0.10 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 4002 FR  Polyphthalamide (PPA) Glass Fiber 15% - Flame Retardant
RTP Company RTP 4002 FR A HS Polyphthalamide (PPA), Glass Fiber - Flame Retardant - Heat Stabilized
RTP Company RTP 4002 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant

PQZWA3264 / 91610

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.