MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Matexcel GRA-A001 Graphene Additives for Construction
Categories: Wood and Natural Products

Material Notes: Graphene additive can be easily dispersed into admixture and additive formulations or water prior to mixing with cement, sand and aggregates, similar to any typical reagent or additive. With dosage rates as low as 0.01% of total concrete mix, a small amount of graphene additives goes a long way when it comes to enhancing strength, durability and multifunctionality. This enables thinner, lighter concrete products with improved tensile and compressive strength, reducing the carbon footprint of construction. Thisproduct also can be used across many other applications, such as paints, inks, latex, polymer and cement composites.

Application: Sectors Construction, automotive, leisure products, textiles, coatings

Morphology: Black Liquid

Key Words: GRA-A001; Graphene Additives for Construction; graphene cement, graphene concrete
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 20.0 °C
 
Descriptive Properties
Product overviewGraphene Additives for Construction is predispersed in water and the concentration of graphene is 20%wt. The average particle size of graphene is 10-20µm.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK2156 / 300787

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.