MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 50 H2 PA6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This product is available in natural & black, and in other colors upon request.

Benefits: This product, UL94 VO @ 0,4mm, offers excellent moldability together with good stiffness.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Connectivity- junction blocks, terminal blocks, connectors…

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527 Type 1A
Tensile Strength, Yield 50.0 MPaISO 527 type 1 A
Elongation at Break 38 %ISO 527 Type 1A
Elongation at Yield 5.0 %ISO 527 type 1 A
Tensile Modulus 2000 MPaISO 527 Type 1A
Flexural Strength 70.0 MPaISO 178
Flexural Modulus 2000 MPaISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²ISO 180/1eA
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 3.9IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243
Dissipation Factor 0.060IEC 60250
Comparative Tracking Index 60 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0
Domo TECHNYL® C 50 H2 PA6, DRY
Teknor Apex Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced
PlastxWorld Veroplas PA2001F Nylon 6
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant

PRHOD790 / 138021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.