MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Luriblend® POM CO GF10 TL10 BK 10% Glass Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 10% Glass Fiber Reinforced; Acetal Copolymer, PTFE Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 10% Filler by Weight

Additive: PTFE Lubricant(10%)

Features: Lubricated, Copolymer, Good Wear Resistance and Low Friction

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.012 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength, Yield 10500 psiASTM D638
Elongation at Break 2.5 %ASTM D638
Flexural Strength 17000 psiASTM D790
Flexural Modulus 620000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Strength 450 V/milMethod A (Short-Time); ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 37.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 335 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 325 °FUnannealed; ASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® GC10 POM, 10% Glass Reinforced
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled
Celanese Celcon® GC10TF 10% Glass Fiber Reinforced, Coupled Acetal Copolymer
Avient Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66)
RTP Company RTP 800 GB 10 TFE 15 Acetal (POM) Glass Bead - PTFE Lubricated

PTPC0874 / 136812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.