MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Dry)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced; Nylon (Polyamide PA)

Material Notes: Terblend® N NG-02 EF is an 8% glass fiber reinforced UV-stabilized ABS/PA blend with enhanced dimensional stability, rigidity and high flowability. High dimensional stability, Excellent flow for high surface quality appearance, Enhanced softening temperature, Enhanced rigidity, UV-stabilized.

Applications: Automotive parts, Motorcycle fairings, Truck cabin parts

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Filler Content 8.0 %
Moisture Absorption at Equilibrium 1.1 %
@Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 2577
Melt Flow 40 g/10 min
@Load 10.0 kg,
Temperature 240 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaISO 527
Elongation at Break 6.0 %ISO 527
Elongation at Yield 3.0 %ISO 527
Tensile Modulus 3100 MPaISO 527
Flexural Strength 85.0 MPaISO 178
Flexural Modulus 2800 MPaISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 12.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.018
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 130 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 118 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 200 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 270 °CISO 294
Mold Temperature 40.0 - 80.0 °CISO 294
 
Descriptive Properties
ColorNatural
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, DAM
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned
Covestro Bayblend® T85 XF Polycarbonate + ABS
INEOS Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Conditioned)

PBASG0602 / 132235

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.