MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 6253 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD Chemlok® 6253 adhesive is a one-coat adhesive used to bond a variety of vulcanized and unvulcanized rubber compounds to metal. It is formulated without heavy metals and composed of a mixture of polymers, organic compounds and mineral fillers dissolved or dispersed in an organic solvent system. A single coat of Chemlok 6253 adhesive will bond compounds based on natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR), nitrile (NBR), butyl (IIR) and EPDM polymers to metal. These mechanically or chemically treated metals include carbon and alloy steels, stainless steel, aluminum, magnesium, zinc, copper and copper alloys. For maximum protection or when environmental conditions are severe, Chemlok 6253 adhesive can be used over Chemlok 205 primer or Chemlok 207 primer.

Features: applies easily by spray, dip or brush methods. requires only a single coat for most applications, reducing labor, solvent usage, inventory and shipping costs; contains higher solids content, allowing for greater square footage coverage per gallon used. provides excellent resistance to various elements. formulated without heavy metals. accommodates a wide range of processing conditions at moderate temperatures, including extended prebake.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.40 - 8.80 lb/gal
Solids Content 28.5 - 32.5 %by weight
Brookfield Viscosity 250 - 800 cP
@Time 25.0 - 85.0 sec
Brookfield LVT, Spindle 2, 30 rpm, Zahn Cup #3
 
Thermal PropertiesOriginal ValueComments
Flash Point 27.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9008 / 232397

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.