MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Avient Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of competition. When specified, Trilliant® compound may incorporate agency rated materials that meet USP Class IV, FDA or ISO 10993 testing requirements. This Trilliant® grade is a high density specialty compound featuring a sustainable material solution for radiation shielding and weighting & balancing applications. The composite material offers a high performance thermoplastic-based alternative to lead. This compound has densities similar to traditional metals and provides greater flexibility in design and processing.

Shielding properties: Attenuation coefficient at 511 keV = 0.83cm-1 Half Thickness at 511 keV = 0.84cm

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccISO 1183
Linear Mold Shrinkage 0.0050 - 0.015 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ISO 868
Tensile Strength at Break 3.00 MPaISO 37
Elongation at Break 200 %ISO 37
Compression Set 20 - 30 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 80 - 90 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+6 - 1.00e+9 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.00 - 2.00 W/m-KThrough Plane; ASTM E1461
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 220 °C
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 80.0 °C
Dry Time 4.00 hour
 
Descriptive Properties
AppearanceGrey
FeaturesHigh Specific Gravity
 Non-Toxic
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesHousings
 Medical/Healthcare Applications
 Radiation Shielding
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Avient Trilliant™ HC 5410-0030RS Natural Polyethylene, High Density (HDPE)
Eastman Tritan™ TX1000 Copolyester
Daikin DAI-EL® T-530 Thermoplastic Fluoroelastomer
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber

PH0POL1319 / 145888

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.