MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:
  • This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.
  • Improved dimensional stability, recyclability, and increased stiffness.
  • Good Z direction properties and an excellent choice for applications requiring reduced weight and higher temperatures.

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.370 g/cc0.0134 lb/in³ASTM D1895
Density 0.820 g/cc0.0296 lb/in³Sintered; ASTM D792
Particle Size 55 µm55 µmD50
 35 - 100 µm35 - 100 µmD10-D90
Melt Flow 26 g/10 min
@Load 5.00 kg,
Temperature 235 °C
26 g/10 min
@Load 11.0 lb,
Temperature 455 °F
3 min; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 33.0 MPa4790 psiZ; ASTM D638
 49.0 MPa7110 psiXY; ASTM D638
Elongation at Break 3.0 %3.0 %XY; ASTM D638
 3.0 %3.0 %Z; ASTM D638
Tensile Modulus 1.945 GPa282.1 ksiZ; ASTM D638
 3.816 GPa553.5 ksiXY; ASTM D638
Flexural Modulus 4.313 GPa625.5 ksiZ; ASTM D790
 5.04 GPa731 ksiXY; ASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 760000 ohm-cm760000 ohm-cmASTM D257
Surface Resistance 40000 ohm40000 ohm
 
Thermal PropertiesMetricEnglishComments
Melting Point 184 °C363 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsamid® AZM 30 BLACK T6LD PA12-GF30
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Haysite H208 Polyester, Magnetic Permeable
Norplex-Micarta SP525M (WaveMax 5000) Glass Fabric
Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled

PALP87 / 177148

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.