Hostalen GM 5010 T3 black is a high density polyethylene (HDPE), black colored similar RAL 9004 with high melt viscosity for extrusion, injection and compression molding. The product is classified as PE 80 and provides excellent stress crack resistance properties (ESCR) combined with very good long term hydrostatic strength. Applications: Drinking Water Pipe, Gas Pipe, Industrial, Soil & Waste PipeInformation provided by LyondellBasell. |