Encom Polymers EnLast 65A TPV
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Vulcanizate Elastomer (TPV)
Material Notes:
Appearance: Black
Processing Methods: Injection Molding
Applications: Automotive, Appliance, General Industrial
Information provided by EnCom Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.03
g/cc
1.03
g/cc
Method A; ISO 1183
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
65
65
15 sec delay; ISO 868
66.3
66.3
1008 Hours at 100°C in an air circulating oven followed by indicated property testing at 23°C; ISO 188
Tensile Strength, Yield
3.80
MPa
551
psi
Type 1, 50mm/min; ISO 37
4.142
MPa
600.7
psi
1008 Hours at 100°C in an air circulating oven followed by indicated property testing at 23°C; ISO 188
Elongation at Break
415 %
415 %
Type 1, 50mm/min; ISO 37
452.35 %
452.35 %
1008 Hours at 100°C in an air circulating oven followed by indicated property testing at 23°C; ISO 188
Tear Strength
21.0
kN/m
120
pli
Method B, Procedure b, 50mm/min; ISO 34-1
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
160
-
182
°C
320
-
360
°F
Middle Barrel Temperature
171
-
193
°C
340
-
380
°F
Front Barrel Temperature
182
-
204
°C
360
-
400
°F
Nozzle Temperature
182
-
204
°C
360
-
400
°F
Melt Temperature
193
-
204
°C
380
-
400
°F
Mold Temperature
32.2
-
71.1
°C
90.0
-
160
°F
Back Pressure
0.172
-
0.689
MPa
25.0
-
100
psi
Vent Depth
0.00127
-
0.00381
cm
0.000500
-
0.00150
in
Screw Speed
25
-
75
rpm
25
-
75
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PENCOM215 / 266229
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.