3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package testing, power electronics and computer cooling. Features and Benefits - Thermal stability
- Chemical stability
- Wide liquid range
- Non-conductive
- Narrow boiling range
- Compatibility
Information provided by 3M |