MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 5250-4 BMI Prepreg System with Woven Glass Fiber 6781
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: CYCOM® 5250-4 is a 350°F to 400°F (177°C to 204°C) curing bismaleimide resin with a service temperature range of -75°F to 400°F (-59°C to 204°C). CYCOM 5250-4 is specifically formulated for use in primary aircraft structures. In addition, a variety of secondary structural components can take advantage of the increased performance from using high-strain carbon fibers and the improved damage-resistance this system provides. CYCOM 5250-4 is available with either carbon fiber or glass fiber reinforcement in unidirectional tape, woven broadgood and roving forms.

Features & Benefits:

  • Short-term service temperature up to 450°F (232°C)
  • Superior hot/wet properties at 220°F to 375°F (104°C to 190°C)
  • Excellent toughness
  • Void-free laminates
  • High temperature resistance
  • Low thermal conductivity
  • Versatile cure
  • Excellent compression strength properties after impact
  • Shop life greater than 28 days at room temperature
  • Fluid/solvent resistant
Suggested Applications: Primary and secondary aircraft structure including:
  • Engine nacelles
  • Fuselage skins and stiffeners
  • Wing and stabilizer spars and skins
  • Other critical load-bearing components
Mechanical properties are reported for standard cure + standard post-cure

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 2.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 86000 psi
@Temperature 24.0 °C
Warp, Glass Style 6781; ASTM D638
Tensile Modulus 27.6 GPa
@Temperature 24.0 °C
Warp, Glass Style 6781
Compressive Strength 497 MPa
@Temperature 24.0 °C
Warp, Glass Style 6781; ASTM D695
Compressive Modulus 25500 MPa
@Temperature 24.0 °C
Warp, Glass Style 6781
Shear Strength 9000 psiShort Beam Warp, Glass Style 6781; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °FContinuous; depends on cure cycle
 450 °Fshort term; depends on cure cycle
Minimum Service Temperature, Air -75.0 °F
Glass Transition Temp, Tg 200 °CWet; QC-PT-22
 216 °CPost Cure: 177°C for 6 hrs
 249 °CPost Cure: 190°C for 6 hrs
 263 °CPost Cure: 210°C for 6 hrs
 282 °CPost Cure: 227°C for 6 hrs
 300 °CDry; QC-PT-22
 304 °CPost Cure: 243°C for 6 hrs
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 - 400 °FCure Temperature - Autoclave
Gel Time 65.0 min
@Temperature 177 °C
in nitrogen atmosphere; QC-TP-87
Shelf Life >= 1.00 Month
@Temperature 72.0 °C
 >= 3.00 Month
@Temperature 4.44 °C
 >= 12.0 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 6781 Fiber Glass Fabric
Solvay CYCOM® 5320-1 Epoxy with T40/800B Unidirectional Tape Composite
Solvay CYCOM® 5250-4 BMI Prepreg System with G30-500-3K-8HS Woven Carbon Fiber
Solvay CYCOM® 5250-4 BMI Prepreg System with G30-500-3K-70PW Woven Carbon Fiber
Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber

PCYTED133_8 / 192684

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.