MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei Stylac™ 181 ABS Polymer, High Heat Resistant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes:

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 9.99 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103
@Thickness 2.50 mm
Tensile Strength, Yield 45.0 MPa50mm/min; ISO 527-1
Flexural Strength 74.0 MPa2mm/min; ISO 178
Flexural Modulus 2350 MPa2mm/min; ISO 178
Charpy Impact, Notched 22.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °CRelative Thermal Index; UL 746A
Hot Ball Pressure Test 100 °CRegistered Number: B-1564; EMAC
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °CISO 75-1,2
Vicat Softening Point 108 °C
@Load 5.10 kg
ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
Möller Medical PolySkin 82 NanoCoating
Ineos ABS Lustran® 488
Avient Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS)

PASAHI8269 / 221293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.