MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound EC006APQ Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP THERMOCOMP EC006APQ compound is based on Polyetherimide (PEI) resin containing 30% carbon fiber. Added features of this grade include: Electrically Conductive, High Flow, FAR25.853 Compliant.

Features: FAR 25.853 Compliant,High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),High Flow,Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.110 %0.110 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 cm/cm0.0010 in/in24hrs; ASTM D955
Melt Flow 69 g/10 min
@Load 6.70 kg,
Temperature 380 °C
69 g/10 min
@Load 14.8 lb,
Temperature 716 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 252 MPa36500 psi5 mm/min; ISO 527
 281 MPa40800 psi5 mm/min; ASTM D638
Elongation at Break 1.1 %1.1 %5 mm/min; ISO 527
 1.1 - 1.3 %1.1 - 1.3 %5 mm/min; ASTM D638
Tensile Modulus 29.25 GPa4242 ksi1 mm/min; ISO 527
 30.52 GPa4427 ksi5 mm/min; ASTM D638
Flexural Strength 332 MPa48200 psiISO 178
 350 MPa50800 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 23.93 GPa3471 ksi2 mm/min; ISO 178
 26.3 GPa3810 ksi1.3 mm/min, 50 mm span; ASTM D790
Compressive Strength 231 MPa33500 psiSABIC method
Poissons Ratio 0.440.44ASTM E132
Shear Modulus 4.726 GPa685.5 ksiASTM D732
Shear Strength 128 MPa18600 psiASTM D732
Izod Impact Notched 82.0 J60.5 ft-lbASTM D256
Izod Impact, Unnotched 7.13 J/cm13.4 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 ohm1000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 5.00 µm/m-°C
@Temperature -40.0 - 150 °C
2.78 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow 7.00 µm/m-°C
@Temperature -40.0 - 150 °C
3.89 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
@Thickness 3.20 mm
383 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 390 - 400 °C734 - 752 °F
Zone 2 370 - 390 °C698 - 734 °F
Zone 3 380 - 400 °C716 - 752 °F
Melt Temperature 360 - 400 °C680 - 752 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81578 / 289525

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.