System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ascend Performance Materials Starflam® RF0052E PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6/66
Material Notes:
Starflam RF0052E is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding Resin
Former Eurostar product. Eurostar has been acquired by Ascend Performance Materials.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.37
g/cc
DAM; ISO 1183
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
120
MPa
DAM; ISO 527-2
Elongation at Break
2.7 %
DAM; ISO 527-2
Tensile Modulus
8100
MPa
DAM; ISO 527-2
Flexural Strength
185
MPa
DAM; ISO 178
Flexural Modulus
6700
MPa
DAM; ISO 178
Izod Impact, Notched (ISO)
6.00
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO)
40.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Electrical Properties
Original Value
Comments
Arc Resistance
120
-
180
sec
@Thickness 3.00 mm
PLC 5; ASTM D 495
Comparative Tracking Index
400
-
599
V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI
7.0
-
15
sec
PLC 4; UL 746
60
-
120
sec
UL 746
>=
120
sec
PLC 0; UL 746
High Amp Arc Ignition, HAI
60
-
120
arcs
PLC 1; UL 746
>=
120
arcs
PLC 0; UL 746
>=
120
arcs
PLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR
25.4
-
80.0
mm/min
PLC 2; UL 746
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
251
°C
Unannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi)
215
°C
Unannealed; DAM; ISO 75-2/A
UL RTI, Electrical
65.0
°C
@Thickness 0.800 mm
UL 746
65.0
°C
@Thickness 1.60 mm
UL 746
65.0
°C
@Thickness 3.20 mm
UL 746
UL RTI, Mechanical with Impact
65.0
°C
@Thickness 0.800 mm
UL 746
65.0
°C
@Thickness 1.60 mm
UL 746
65.0
°C
@Thickness 3.20 mm
UL 746
UL RTI, Mechanical without Impact
65.0
°C
@Thickness 0.800 mm
UL 746
65.0
°C
@Thickness 1.60 mm
UL 746
65.0
°C
@Thickness 3.20 mm
UL 746
Flammability, UL94
V-2
@Thickness 0.800 mm
V-2
@Thickness 1.60 mm
V-2
@Thickness 3.20 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
265
-
275
°C
Injection
Middle Barrel Temperature
265
-
275
°C
Injection
Front Barrel Temperature
270
-
280
°C
Injection
Melt Temperature
270
-
280
°C
Injection
Mold Temperature
60.0
-
100
°C
Injection
Drying Temperature
80.0
°C
Injection
Dry Time
4.00
hour
Injection
Moisture Content
0.20 %
Injection
Descriptive Properties
Additive
Flame Retarding Agent
Heat Stabilizer
Release agent
Agency Ratings
ISO, 1043 PA66+PA6 GF25 FR(30)
Appearance
Natural Color
Features
Flame Retardant
Forms
Pellets
Processing Method
Injection Molding
Region
North America, Europe
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6
Overview of materials for Nylon 66/6, Mineral Reinforced
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant
Grupo Repol Dinalon® C1S25 PA6/PA66 Blend, Unreinforced
PEUROSTA45 / 172059
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.