MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 279 Mixture of acetylacetone peroxide and tert-butyl peroxybenzoate in solvents
Categories: Other Engineering Material

Material Notes: Trigonox 279 is a fast peroxide blend for the cure of unsaturated polyester resins at elevated temperatures in combination with a cobalt accelerator.

CAS number: 614-45-9, 37187-22-7

EINECS/ELINCS No: 210-382-2; 253-384-9

Applications: Trigonox 279 is a peroxide formulation based on acetylacetone peroxide and tert butyl peroxybenzoate. Trigonox 279 has specially been developed for the cure of unsaturated polyester resins at elevated temperatures in combination with a cobalt accelerator (e.g. Accelerator NL-49 PN = 1% cobalt). Application area for the cure system Trigonox 279 plus a cobalt accelerator can be e.g. continuous laminating, resin transfer molding, filament winding and centrifugal casting.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.054 g/cc
Storage Temperature -5.00 - 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Color= 100 Pt-Co / APHA
Content4.3-4.7 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1084 / 286607

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.