MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Lubri-Tech™ AT-10CF/15T-2S Acetal-Copolymer, Carbon Fiber Reinforced, PTFE/Silicone Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes:

Description/Features:

  • Carbon Fiber Reinforced
  • PTFE/Silicone Lubricated
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Water Absorption 0.18 %
@Thickness 3.17 mm
0.18 %
@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 79.3 MPa11500 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %3.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 5.17 GPa750 ksiType 1 - Rigids, 0.2 in/min; ASTM D638
Izod Impact, Notched 0.507 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.950 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 - 10000 ohm-cm1000 - 10000 ohm-cmASTM D257
 
Processing PropertiesMetricEnglishComments
Melt Temperature 188 - 210 °C370 - 410 °FMolding
Mold Temperature 54.4 - 82.2 °C130 - 180 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2 hour2 hour
 
Descriptive Properties
Product FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
Avient Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
Avient LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer
Avient LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer
Avient LubriOne™ ATH-000/05T Acetal (POM) Homopolymer

PH1PO0148 / 43397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.