MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Silastic® NPC 9300-70 LSR Non-Post-Cure Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: SILASTIC™ NPC 9300 Series LSRs are low-volatility, high-strength silicone elastomers formulated to meet the requirements of food and infant care regulated applications without the need for post-cure.

Product applications:

  • Infant care (soothers, nipples)
  • Food contact (cookware, valves, diaphragms)
  • General consumer articles
Key Features:
  • Low volatile content
  • Eliminates post-cure operations
  • Enables streamlined processes and part design flexibility
  • High strength Unique rheology
  • Low modulus

Former Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Volatiles 0.25 %EN 1400:2013; EN 14350-2:2004
Viscosity 210000 cP
@Frequency 10 Hz
Part B; CTM 1094
 220000 cP
@Frequency 10 Hz
Part A; CTM 1094
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67ASTM D2240
Tensile Strength 9.60 MPaASTM D412
Elongation at Break 320 %ASTM D412
Tear Strength 27.0 kN/mASTM D624 DIE B
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Contact; FDA 21 CFR 177.2600

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Silastic® HV 1551-95P LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® HV 1523-30 LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® HV 1519-40 LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® HV 1510-40 LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® DY-35-3115 Liquid Silicone Rubber

PDOW9918 / 233121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.