MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Lustran® PG298 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Lustran® PG298 resin is a grade of ABS (acrylonitrile butadiene styrene) for use in automotive and general-purpose applications. It provides a unique combination of flow and rigidity, with increased scratch resistance. SAE J1685:ABS0111, Plating grade, Improved thermocycle performance, Outstanding plate adhesion, Increased scratch resistance Applications: Grills, Wheel covers, Mirror housings, Appliance, lawn and garden

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D 955
Melt Flow  5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
 19 g/10 min
@Load 10.0 kg,
Temperature 220 °C
19 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D 785
Tensile Strength, Yield 40.0 MPa5800 psiASTM D 638
Tensile Modulus 2.77 GPa402 ksiASTM D 638
Flexural Strength 78.3 MPa11400 psiASTM D 790
Flexural Modulus 2.83 GPa410 ksiASTM D 790
Izod Impact, Notched 1.71 J/cm
@Temperature 23.0 °C
3.20 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °Funannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 83.9 °C183 °Funannealed; ASTM D 648
Vicat Softening Point 110 °C
@Load 1.02 kg
230 °F
@Load 2.25 lb
B/2 120C/H; ASTM D 1525
 
Processing PropertiesMetricEnglishComments
Drying Temperature 79.0 °C
@Time 7200 - 14400 sec
174 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® MP-0160R Metal Plating Grade ABS
INEOS Styrolution Novodur® P2MC Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® 433 Acrylonitrile Butadiene Styrene (ABS)
Proto Labs Aluminum AlSi10Mg - DMLS
INEOS Styrolution Lustran® 308 NR Acrylonitrile Butadiene Styrene (ABS)

PSTYR9853 / 216080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.