MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Haysite Dura-Core 1000 Composite Panel
Categories: Polymer

Material Notes: Haysite Reinforced Plastics grade Dura-Core 1000™ is engineered for use as a floor material in light transit rail car interiors and multi-wheeled vehicle applications. The compression molded composite panel combines high strength fiberglass reinforced plastic (FRP) laminate skins with a lightweight thermoplastic foam core material. The panel exhibits excellent flame, smoke, and toxicity properties (FST) that meet stringent transit industry specifications for FST and is halogen free.

Dura-Core 1000 is compression molded in a ‘sandwich’ core construction yielding a strong, durable, one-piece composite. The composite system’s physical properties also offer excellent corrosion and chemical resistance; providing very low moisture absorption and excellent resistance to a variety of harsh weather environments.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.630 g/ccComposite; ASTM D792
 9.40 lb/ft³Core; ASTM D1622
Water Absorption 0.51 %Composite; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 57Composite; ASTM D2583
Tensile Strength 340 psiComposite Flatwise; ASTM C297
Compressive Strength 261 psiCore; ASTM D1621
 1250 psiComposite Flatwise; ASTM C365
Shear Modulus 23.5 ksiComposite; ASTM C273
Shear Strength 280 psiComposite Flatwise; ASTM C273
Peel Strength 19.4 pliDrum Peel; Composite; ASTM D1781
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
 
Descriptive Properties
Fire Test> 42 minutesUnloaded; ASTM E119
Radiant Panel - Flame Spread80 secondsIgnition Time, ASTM D229
Surface Flammability11.79ASTM E162
Toxicity TestCarbon Monoxide180 ppm, Passes BSS 7239
 Hydrogen Chloride1.0 ppm, Passes BSS 7239
 Hydrogen Cyanide0 ppm, Passes BSS7 239
 Hydrogen Fluoride0.5 ppm, Passes BSS 7239
 Nitrogen Dioxide10.5 ppm, Passes BSS 7239
 Sulfur Dioxide0 ppm, Passes BSS 7239

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAY517f / 238965

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.