MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo Plexiglas® MI7 Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Plexiglas® MI7 is an impact modified thermoplastic acrylic resin formulated for injection molding and extrusion applications. It is heat resistant, has high melt flow and provides 7 times the impact resistance of standard acrylics while maintaining excellent optical properties. It offers an excellent balance between melt flow and increased resistance to breakage, while providing weatherability superior to that provided by other high-impact plastics. Supplemental moldflow simulation data is available.

Appearance: Clear/Transparent; Colors Available; Opaque; Translucent

Characteristics: High Heat Resistance; High Clarity; Scratch Resistant; Good Color Stability; Good Dimensional Stability; Low Shrinkage; Good Thermal Stability; Good UV Resistance; Good Weather Resistance; Good Toughness; Medium Impact Resistance; Good Flow

Applications: Automotive Exterior Parts; Lighting Diffusers

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Water Absorption 0.30 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmASTM D955
Melt Flow 3.2 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 68ASTM D785
Tensile Strength, Ultimate 7000 psiASTM D638
Elongation at Break 35 %ASTM D638
Tensile Modulus 365000 psiASTM D638
Flexural Strength <= 11200 psiASTM D790
Flexural Modulus 345000 psiASTM D790
Izod Impact, Notched 0.600 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.40 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 196 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 185 °Fannealed; ASTM D648
Vicat Softening Point 194 °F50°C/hr; 50N; ASTM D1525
 210 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Temperature 22.8 °C
ND; ASTM D542
Haze <= 2.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 91 %
@Thickness 3.17 mm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Plexiglas® DR® Acrylic
Trinseo Plexiglas® V920 Acrylic
Trinseo Plexiglas® SG7 Acrylic
Trinseo Plexiglas® V825 Acrylic
Trinseo Plexiglas® V826 Acrylic

PARKG039 / 24393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.