MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® G1750X (EP)n Multi-Arm Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: (EP) ethylene/propylene multi-arm (branched) copolymer. "X" denotes developmental product. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact qualities of the material, both at room and low temperature. This KRATON polymer meets FDA regulations as articles or as ingredients in articles intended for food contact. FDA clearances vary from one grade to another. For specific clearances, letters of certification will be provided on request.

Applications: modified asphalts, thermoplastic and thermoset polymer modification, adhesives, sealants, coatings, oil gels, and general elastomer compounding.

Information provided by the manufacturer, Kraton® Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.860 g/cc
Brookfield Viscosity 8700 cP
@Temperature 25.0 °C
Toluene solution. Neat polymer concentration, 25%w.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 1110 seconds. Typical values on polymer compression molded at 150°C (300°F).
Tensile Strength, Ultimate <= 0.345 MPaTypical properties based on film cast from toluene solution. Tensile tester jaw separation 10 in/min (25.4 cm/min); ASTM D412
Elongation at Break 100 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm
Dielectric Strength 11.81 - 39.37 kV/mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 260 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® G1765X (EP)n Multi-Arm Copolymer
Kraton® FG1924 G (SEBS) Linear Block Copolymer
Kraton® G1650 E (SEBS) Linear Block Copolymer
Kraton® G7723X
Kraton® G1780X (SEP)n Multi-Arm Copolymer

PKRA0310 / 49091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.