MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M3700  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 112 cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79ASTM D2240
Tensile Strength, Yield 43.4 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 35 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2380 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 71.0 MPaASTM D790
Flexural Modulus 2480 MPaASTM D790
Izod Impact, Notched 26.7 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Injection Molded; ASTM D256A
 107 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Injection Molded; ASTM D256A
 374 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 75.0 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 72.8 °C
@Thickness 6.35 mm
Annealed; ASTM D648
UL RTI, Electrical 90.0 °CUL 746
UL RTI, Mechanical with Impact 85.0 °CUL 746
UL RTI, Mechanical without Impact 90.0 °CUL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
All Colors; CSA
 V-0
@Thickness 1.50 mm
All colors; UL 94
 5VA
@Thickness 1.57 mm
All Colors; CSA
 5VA
@Thickness 1.80 mm
All colors; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Descriptive Properties
Agency RatingsNSF 51
 NSF 61
FeaturesGeneral Purpose
 High Flow
 Medium Impact Resistance
FormsPellets
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliances
 Business Equipment
 Construction Applications
 Electrical/Electronic Applications
 General Purpose
 Telecommunications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid
Borealis RA130E-2491 Polypropylene Random Copolymer
Dow HDPE 17450N High Density Polyethylene
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Chi Mei Polylac® PA-709 ABS

PH1PN8836 / 102672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.