Application: Copolymerization in emulsion and solution. Used as internal plasticizer. Also used in oil additives as well as in the leather, textile, paint, and paper industries. Appearance: Clear and colorless liquid Odor: Ester-like CAS: 688-84-6 Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale. |