MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parson Adhesives PARTITE® 9330 Acrylic Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 9330 a no-mixing, high viscosity combined with medium cure speed structural adhesive for wide variety of industrial assembly applications. It bonds wide range of materials with the use of Activator 1649.

FEATURE:

  • Adhesive is applied to one surface and Activator to the other; press together and fixing is achieved within few minutes.
  • Excellent resistance to gasoline, lubricants, water, solvents, etc.
APPLICATIONS:
  • Ideal for bonding Metals, Ferrite, Plated Metals, Ceramic, Wood, etc.
  • Widely used for tool handle, electric motors, loudspeaker, decorative articles, sporting goods, appliances, etc.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Brookfield Viscosity 45000 - 80000 cPRVT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1800 psiISO 37
Elongation at Break 90 %ISO 37
Tensile Modulus >= 44000 psiASTM D638
Shear Strength >= 2175 psiSteel to Steel, grit blasted; ISO 4587
Peel Strength >= 11.0 pliISO 11339
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.5DIN 53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 275 °F
Minimum Service Temperature, Air -65.0 °F
Flash Point >= 92.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 7.00 minSpeed
 24.0 hourFull
 
Descriptive Properties
ColorPale Yellow liquid
CompositionUrethane Methacrylate
Gap Filling0.05-0.7 mmCured
Initial Strength Retained (%)100Motor Oil for 500 hrs at 22°C
 100Motor Oil for 1000 hrs at 22°C
 40Water/Glycol for 500 hrs at 22°C
 40Water/Glycol for 1000 hrs at 22°C
 50Acetone for 1000 hrs at 22°C
 55Acetone for 500 hrs at 22°C
 75Ethanol for 1000 hrs at 22°C
 80Ethanol for 500 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN088 / 186531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.