MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt CDA 110 Electrolytic Tough Pitch Copper (AWS BCu-1b)
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy; Pure Element

Material Notes: CDA 110 is a fluid filler metal used for brazing of ferrous and nickel based alloys in particular steel, stainless steel and copper-nickel alloys. This alloy is typically used in a furnace braze applications without the use of flux. CDA 110 is a free flowing filler metal that exhibits good wetting characteristics on ferrous and nickel based materials. Maximum strength and joint integrity are obtained where joint clearance falls within the range of 0.000 in - 0.001 in. (0.000 – 0.025 mm) per side. The properties of a brazed joint are dependent upon numerous factors including base metal properties, joint design, metallurgical interaction between the base metal and the filler metal.

Available forms: Wire, strip, engineered preforms, and specialty preforms.

Information provided by Lucas-Milhaupt.

Key Words: AWS A5.8M/A5.8 BCu-1b; AMS 4500 (Chemistry Only)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.94 g/cc8.94 g/cc
Density 8.94 g/cc0.323 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000171 ohm-cm0.00000171 ohm-cm101% IACS
 
Thermal PropertiesMetricEnglishComments
Melting Point 1083 °C1981 °F
Solidus 1083 °C1981 °F
Liquidus 1083 °C1981 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1090 - 1180 °C2000 - 2150 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.9 %>= 99.9 %
Other, total <= 0.10 %<= 0.10 %
 
Descriptive Properties
ColorCopper

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NLUCM9812 / 254758

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.