MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow VORANOL™ CP 6001 Polyol
Categories: Polymer; Thermoset

Material Notes: VORANOL™ CP 6001 polyol is a triol polyether polyol, capped, specially developed for the production flexible HR molded polyurethane foam with TDI, TDI/PMDI or MDI. It can be used in the production of semi-rigid integral skin foams as well as in the production of cold cure molded foams and high resilience molded.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.022 g/cc
pH 8.0 - 9.5(1 Water / 10 Methanol); DOWM 101495-TE94A
Viscosity Measure 370 cSt
@Temperature 50.0 °C
ASTM D445-94
 600 cSt
@Temperature 37.8 °C
ASTM D445-94
 1060 - 1200 cSt
@Temperature 25.0 °C
ASTM D445-94
Molecular Weight 6000 g/mol
Maximum Moisture Content 0.060wt% water; ASTM E203-96
ASTM Color <= 30APHA; ASTM D4890-93
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.050[mg KOH/g]; DOWM 100387-TE95A
 
Thermal PropertiesOriginal ValueComments
Flash Point 240 °CC.O.C. (open cup)
 
Descriptive Properties
Hydroxyl Number mg KOH/g26 - 29ASTM D4274-94d

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow VORANOL™ CP 4711 Polyol
Dow VORANOL™ CP 1421 Polyol
Dow VORANOL™ CP 755 Polyol
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
Dow VORANOL™ 4701 Polyether Polyol

PDOW1480 / 30698

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.