MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® FR6901 Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded; Polycarbonate, Unreinforced, Flame Retardant; Polycarbonate, UV Stabilized

Material Notes: Main characteristics:
• High toughness
• Good heat resistance
• Glass-like transparency, optical quality
• High dimensional accuracy and stability

Grade characteristics:
• Flame retardant
• High reflectance
• Low viscosity, easy release
• UV stabilized

Formerly Makrolon DP1-1890

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.12 %ISO 62, 50% RH
Water Absorption at Saturation 0.30 %ISO 62
Melt Flow 18.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-1,-2
Tensile Modulus 2400 MPa1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Thickness 3.20 mm,
Temperature 23.0 °C
complete break; b.o. ISO 180-A
 12.0 kJ/m²
@Thickness 3.20 mm,
Temperature -30.0 °C
complete break; b.o. ISO 180-A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.00080
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Vicat Softening Point 143 °C
@Load 5.10 kg
50°C/h; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-1
@Thickness 1.20 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
Flash Point 480 °CASTM D 1929
 550 °Cself ignition; ASTM D 1929
Oxygen Index 36 %Method A; ISO 4589-2
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 93 %
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection molding; ISO 294
Mold Temperature 80.0 °CInjection molding; ISO 294
Injection Velocity 200 mm/secISO 294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade
Covestro Bayblend® FR3010 HF PC/ABS Blend
Covestro Makrolon® 2467 Polycarbonate
Covestro Makrolon® 6165 X Polycarbonate
Covestro Makrolon® 6255 Polycarbonate

PB09657 / 150789

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.