Petrothene NA960 is a series of resins selected for use in a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good uniformity, ease of processing and good tensile strength. Resin : Low Density PolyethyleneInformation provided by LyondellBasell. |