MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Americas Styrenics Styron® 685P Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applications. When used unmodified for the manufacture of food contact articles STYRON 685P complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The regulations should be consulted for complete details.

Data provided by Dow Chemical.

Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM Data
Linear Mold Shrinkage 0.0050 cm/cm
Melt Flow 2.2 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 52.4 MPaASTM Data
Tensile Strength, Yield 52.4 MPaASTM Data
Elongation at Break 2.2 %ASTM Data
Elongation at Yield 2.0 %ISO Data
Tensile Modulus 3.20 GPaASTM Data
Charpy Impact Unnotched 0.800 J/cm²ISO Data
 1.00 J/cm²ISO Data, Low Temp
Charpy Impact, Notched 0.100 J/cm²ISO Data, Low Temp
 0.300 J/cm²ISO Data
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 83.3 °CUnannealed; ASTM Data
Vicat Softening Point 108 °C
Flammability, UL94 HB
@Thickness 3.20 mm
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %
Transmission, Visible 90 %
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accucomp Polystyrene HS0600L High Impact
Lotte Advanced Materials Starex® SD-0150 ABS, Unreinforced
Denka STYROL MW1 Polystyrene
Bamberger Polymers Bapolan® 6450 Polystyrene Injection Molding Resin
Bamberger Polymers Bapolan® 6403 Polystyrene, Extrusion

PDW174 / 34405

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.