LNP THERMOTUF DF002PSI compound is based on Polycarbonate (PC) resin containing 10% glass fiber. Added features of this grade include: Impact Modified, High Flow, Ductile, Good Chemical Resistance. Features: Impact Modified,Chemical Resistance,High Impact Resistance,High Flow Information provided by SABIC |