MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyLabs U-34 Viscoelastic Slow Recovery Memory PU Foam
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: U-34 polyurethane exhibits extremely slow recovery time and is highly conforming. Memory foam exhibits slow recovery to original form when compressed or distorted. U-34 Viscoelastic PU Foam exhibits low ball rebound for enhanced cushioning. Ideally suited for medical padding, general seating, and wheelchair seating applications.

Information provided by PolyLabs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.120 g/cc0.00434 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.159 MPa23.0 psi
Compressive Strength  0.00552 MPa
@Strain 10 %
0.800 psi
@Strain 10 %
Compression Force Deflection
 0.00689 MPa
@Strain 20 %
1.00 psi
@Strain 20 %
Compression Force Deflection
 0.00758 MPa
@Strain 25 %
1.10 psi
@Strain 25 %
Compression Force Deflection
 0.0138 MPa
@Strain 50 %
2.00 psi
@Strain 50 %
Compression Force Deflection
 0.0951 MPa
@Strain 75 %
13.8 psi
@Strain 75 %
Compression Force Deflection
Tear Strength 0.701 kN/m4.00 pliDie C
Compression Set  1.16 %
@Temperature 25.0 °C
1.16 %
@Temperature 77.0 °F
% of original thickness after 50% set
 1.89 %
@Temperature 70.0 °C
1.89 %
@Temperature 158 °F
% of original thickness after 50% set
 2.1 %
@Temperature 25.0 °C
2.1 %
@Temperature 77.0 °F
% of original deflection after 50% set
 2.56 %
@Temperature 70.0 °C
2.56 %
@Temperature 158 °F
% of original deflection after 50% set

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYLA968 / 265878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.