MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco TDH® SS Oil
Categories: Fluid; Lubricant

Material Notes: Texaco TDH Oil SS delivers value through:
  • Reduced operational costs — Excellent performance in a wide range of ambient and operating temperatures provides year-round improved low temperature hydraulic and transmission responsiveness versus typical John Deere J20C fluids. Eliminates the need to switch fluids between seasons thereby saving substantial operating expense.
  • Longer oil life — Outstanding ability of the synthetic base stock to withstand oxidation at high operating temperatures results in increased service life of the oil.
  • Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions - leading to increased equipment life.
  • Lower inventory cost — One fluid does the job of a full range of mobile hydraulic systems. Can replace multiple products and free up shelf space too!
  • Minimized weather and storage concerns — Protects against rust and corrosion of highly finished precision parts when operating in humid conditions and during seasonal shutdown periods.
  • Reduced downtime — Good compatibility with seals, O-rings, and packing materials maintains their good condition and keeps leakage at a minimum.
  • Smoother operation— By eliminating brake "chatter" and transmission "slip" it assures quiet and efficient action of brakes and transmission.
  • More reliable operation — Formulation keeps metal parts clean and free of varnish and sludge deposits that could result in premature breakdown.

Texaco TDH Oil SS (Transmission-Differential-Hydraulic Fluid) is a truly unique, high quality, synthetic, multifunctional fluid, specially formulated for use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other equipment employing a common fluid reservoir.

Texaco TDH Oil SS is specially designed for operation in all types of weather - both severe winter cold and extreme summer heat. It meets the requirements of both John Deere J20C and J20D specifications. This, combined with excellent oxidation stability, eliminates the need for seasonal oil changes.

Its distinctive orange color provides for easy product identification and leak detection.

Texaco TDH Oil SS is a combination lubricant for modern tractors and similar equipment. It performs many functions, such as lubrication of the transmission and final drive, and serves as a hydraulic fluid to operate power steering units, brakes, implements, and attachments. Texaco TDH Oil SS has a viscosity index much higher than typical multifunctional transmission/hydraulic fluids. This provides excellent flow at low temperatures and good oil film protection at high operating temperatures. Furthermore, Texaco TDH Oil SS:

  • Eliminates brake "chatter" and excessive brake facing wear.
  • Assures smooth operation of clutch packs and wet brakes.
  • Provides excellent shifting action.
  • Provides superior rust and corrosion protection for vital parts.
  • Minimizes leakage because of good compatibility with seals, O-rings, and packing materials.
  • Prevents sludge and varnish formation.
  • Protects metal surfaces against scuffing and wear
  • Provides superior gear lubrication compared to typical cold weather, low viscosity tractor hydraulic fluids.
  • Allows for ready leak detection because of its distinctive orange color.

Texaco TDH Oil SS is compatible with other combination tractor, transmission, and hydraulic fluids.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221894; MSDS Number: 8656

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 34.5 °
Brookfield Viscosity 17000 cP
@Temperature -40.0 °C
Viscosity Measurement 204Viscosity Index
Saybolt Viscosity at 100°F 225 SUS
Saybolt Viscosity at 210°F 58.2 SUS
Kinematic Viscosity at 40°C (104°F) 44.7 cSt
Kinematic Viscosity at 100°C (212°F) 9.5 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -45.0 °C
Flash Point 242 °C
 
Descriptive Properties
ColorOrange

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA199 / 77078

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.